| Trade Name | API 5L X60 PSL2 Pipe |
|---|
| Weld Alternatives: | ERW, HF, DSAW/SAWL, SMLS, HSAW |
| OD Size Range: | ERW: 0.375″ through 30″ |
| HF: 0.840″ through 24″ | |
| DSAW/SAWL: 12.75″ through 144″ | |
SMLS: 0.840″ through 26″
HSAW: 8.625″ through 144″ |
| Wall Ranges: | ERW: 0.120″ through 1.000″
HF: 0.120″ through 1.000″
DSAW/SAWL: 0.250″ through 6.000″
SMLS: 0.250″ through 2.500″
HSAW: 0.250″ through 1.000″ |
| Lengths: | Single Random
Double Random
Custom (up to 300′) |
| Grade: | ASTM A53, ASTM A106, ASTM A179, ASTM A192, ST35.8, ST37, ST42, ST52, E235, E355, S235JRH, S275JR, S355JOH, P235TR1, 10#, 20#, 45#, Q235, Q345 |
| Schedule: | SCH5 SCH10 SCH20 SCH30 SCH40 SCH80 SCH120 SCH140 SCH160 SCHXS SCHXXS |
| Surface Finishes: | Bare, Oiled, Mill Varnish, Galv, FBE, FBE Dual, 3LPE, 3LPP, Coal Tar, Concrete Coating and Tape Wrap. |
| End Finishes: | Beveled, Square Cut, Threaded & Coupled. |
| Additional Services: | Internal Coating |
| CHEMICAL COMPOSITION | | | | | | | | | | | |
|---|
| | | | | | | | | | | |
| Mass fraction, based upon heat and product analysis % maximum | CARBON EQUIVALENT a | | | | | | | | | | |
| % MAXIMUM | | | | | | | | | | | |
| Cb | Si | Mnb | P | S | V | Nb | Ti | Other | CEIIW | CEPcm | |
| SEAMLESS & WELDED PIPES | | | | | | | | | | | |
| L320N or X52N | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | e | 0.43 | 0.25 |
| L320Q or X52Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e | 0.43 | 0.25 |
| WELDED PIPE | | | | | | | | | | | |
| L290M OR X52M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e | 0.43 | 0.25 |
| MECHANICAL REQUIREMENTS | | |
|---|
| | |
| Y.S | T.S | ELONGATION |
| Mpa(psi) | Mpa(psi) | |
| min | min | min |
| 415(60 200) | 565(81 900) | f |
| IMPACT TEST | |
|---|
| |
| AVG. ABSORBED ENERGY | IND. ABSORBED ENERGY |
| Min.(joules) | Min.(joules) |
| 27 | 20 |
| API 5L X60 | (PSL2) |
|---|
| Minimum Yield Strength: | 60,200 psi |
| Maximum Yield Strength: | 81,900 psi |
| Minimum Tensile Strength: | 75,400 psi |
| Maximum Tensile Strength: | 110,200 psi |
| Notes: This is a standard line pipe grade specified in API (American Petroleum Institute) specification 5L. | |
| API 5L X60 Industry Specifications | Chemical Composition | Yield Strength min. (KSI) | Tensile Strength min. (KSI) | Yield to Tensile Ratio (max) | Elongation
% |
|---|---|---|---|---|---|
| ASTM A105, A106, A234, A333, A350, A420, A694,A860 | C 0.16 Si 0.45 Mn 1.65 P 0.020 S 0.010 V 0.08 Nb 0.05 Ti 0.04 | 60 | 75 | 0.93 | 19 |
API 5L X60
Production Standards & Material Qualities
| API 5L L245 / Gr. B (PSL 1)
API 5L L290 / X42 (PSL 1)
API 5L L245 / Gr. B (PSL 2)
API 5L L290 / Gr. B (PSL 2)
API 5L L320 / X46 (PSL 1)
API 5L L320 / X46 (PSL 2) | API 5L L360 / X52 (PSL 1)
API 5L L360 / X52 (PSL 2)
API 5L L415 / X60 (PSL 1)
API 5L L415 / X60 (PSL 2)
API 5L L450 / X65 (PSL 1)
API 5L L450 / X65 (PSL 2) |
|---|---|
| Line Pipe API 5L, PSL 1, PSL 2
CSA Z 245.1
EN ISO 3183
GOST 20295 | Gr A, X70-(N, M)
Gr 241-Gr 359
L 245-L485 (N, M, NE, ME)
K34-K60 |
API 5L X60 PSL2 Pipe features:
API 5L X60 PSL2 Pipe – delivery condition and surface
API 5L X60 PSL2 Pipe – straightness
Ends of the API 5L X60 PSL2 Pipe
Marking of API 5L X60 PSL2 Pipe and tube bundles
API 5L X60 PSL2 Pipe – surface protection
| CHEMICAL COMPOSITION | | | | | | | | | | | |
|---|
| Mass fraction, based upon heat and product analysis % maximum | CARBON EQUIVALENT a | | | | | | | | | | |
| % MAXIMUM | | | | | | | | | | | |
| Cb | Si | Mnb | P | S | V | Nb | Ti | Other | CEIIW | CEPcm | |
| SEAMLESS & WELDED PIPES | | | | | | | | | | | |
| L485Q or X70Q | 0.18f | 0.45f | 1.8f | 0.025 | 0.015 | g | g | g | h | 0.43 | 0.25 |
| WELDED PIPE | | | | | | | | | | | |
| L485M OR X70M | 0.12f | 0.45f | 1.7f | 0.025 | 0.015 | g | g | g | h | 0.43f | 0.25 |
| MECHANICAL REQUIREMENTS | | |
|---|
| Y.S | T.S | ELONGATION |
| Mpa(psi) | Mpa(psi) | |
| min | min | min |
| 485(70 300) | 635(92 100) | f |
| IMPACT TEST | |
|---|
| AVG. ABSORBED ENERGY | IND. ABSORBED ENERGY |
| Min.(joules) | Min.(joules) |
| 27 | 20 |